ISO9001:2015 & IATF16949

Whatsapp:0086-13478609753

Investment Casting Product

Top Quality High Precision Super Alloy Steel Castings

Lantian Precision Machinery Manufacturing company is a large and professional investment casting foundry in China for custom steel castings

SKU: lantian-16-1-1-1-1-1-1 Category: Tag:

Top Quality High Precision Super Alloy Steel Castings

Lantian Precision Machinery Manufacturing company is a China Top 10 investment casting foundry in China, you can get the demanded high precision superalloy steel castings as required. The company is specialized in crafting engineering investment castings more than 30 years meeting your exact specifications and exceed your expectations.

precision investment stainless steel casting stainless steel casting components

What Are Super Alloy Steel Castings?

Super alloy steel castings are using a class of high-performance metallic materials engineered to withstand extreme mechanical stress, high temperatures, and corrosive environments to make a part according to the drawings. Key characteristics include:

  • High-Temperature Strength: Retains mechanical properties at elevated temperatures (up to 1000°C or higher).
  • Corrosion & Oxidation Resistance: Resists degradation in harsh chemical and thermal environments.
  • Excellent Fatigue Resistance: Withstands cyclic loading without failure.
  • Superior Creep Resistance: Maintains structural integrity under prolonged stress at high temperatures.

Common Super Alloy Steel Grades

  • Inconel (e.g., 718, 625, 713LC) – Nickel-based alloys for aerospace turbines.
  • Hastelloy (e.g., X, C-276) – Nickel-molybdenum alloys for chemical processing.
  • Stellite (e.g., 6B, 21) – Cobalt-chromium alloys for wear resistance.
  • Maraging Steel (e.g., Grade 300, 350) – Ultra-high-strength steels for aerospace and defense.

Our Investment Casting Foundry Workflow:

1. Mold Design and Manufacturing
  • Design: Use CAD software to design a 3D model of the casting based on customer requirements.
  • Mold Manufacturing: Manufacture the wax pattern mold using CNC machining.
2. Wax Pattern Production
  • Wax Injection: Inject molten wax into the mold to create a wax pattern that matches the shape of the final casting.
  • Trimming: Trim the wax pattern to remove burrs and defects, ensuring a smooth surface.
3. Wax Pattern Assembly
  • Assembly: Assemble multiple wax patterns into a wax tree to improve production efficiency.
  • Inspection: Inspect the quality of the wax tree to ensure it is defect-free.
4. Shells Production
  • Slurry Dipping: Dip the wax tree into slurry to form a coating.
  • Sand Stuccoing: Sprinkle fine sand onto the wet coating to increase the strength of the shell mold.
  • Drying: Place the coated wax tree in a drying room to dry.
  • Repetition: Repeat the slurry dipping, sand stuccoing, and drying processes until the shell mold reaches the required thickness.
5. Dewaxing
  • Heating: Place the shell mold in a dewaxing furnace to melt and remove the wax pattern.
  • Cleaning: Clean any residual wax inside the shell mold to ensure it is completely clean.
6. Firing
  • Preheating: Preheat the shell mold in a furnace to remove any remaining wax and moisture.
  • High-Temperature Firing: Increase the furnace temperature to a high level to fully sinter the shell mold, enhancing its strength and heat resistance.
7. Melting and Pouring
  • Melting: Melt the steel material in a furnace and adjust its chemical composition to meet the required standards.
  • Pouring: Pour the molten steel into the preheated shell mold for casting.

investment casting production workflow

8. Cooling and Shell Removal
  • Cooling: Allow the casting to cool naturally to room temperature within the shell mold.
  • Shell Removal: Use mechanical or chemical methods to remove the shell mold and extract the casting.
9. Post-Processing
  • Cutting: Cut the casting from the wax tree.
  • Cleaning: Clean the casting surface using methods such as sandblasting or grinding to remove residual ceramic and oxide scale.
  • Heat Treatment: Perform heat treatment, such as quenching and tempering, as needed to improve the mechanical properties of the casting.
  • Machining: Carry out necessary machining to achieve the final dimensions and surface precision.

 

10. Quality Inspection

  • Dimensional Inspection: Use tools such as coordinate measuring machines (CMM) to inspect the dimensional accuracy of the casting.
  • Non-Destructive Testing: Conduct non-destructive testing, such as X-ray or ultrasonic testing, to ensure the casting is free of internal defects.
  • Surface Inspection: Check the surface quality of the casting to ensure there are no cracks, pores, or other defects.
11. Surface Treatment
  • Polishing: Polish the casting surface to improve its smoothness.
  • Coating: Apply coatings, such as electroplating or spraying, as needed to enhance corrosion resistance and aesthetics.
12. Packaging and Shipping
  • Packaging: Perform anti-rust treatment and packaging on qualified castings to ensure they are not damaged during transportation.
  • Shipping: Deliver the packaged castings to the customer’s specified location.
  • Testings We Can Do:

    We have complete testing equipment in our factory. In the aspects of chemical composition test: We have Italy F – 20 direct reading spectrometer, Q6 imported from Germany and domestic spectrometer analysis of the elements C, Si, Mn, P, S, Ni, Cr, Mo, V, Ti, Al, Cu, Mg, Ce, Nb, B, W;

    In the aspect of physical performance testing, we can carry out tensile test, impact test, hardness detection, CMM test etc, metallographic analysis etc.And we have fluorescent magnetic particle detector to do the magnetic particle inspection, ultrasonic inspection and coloring inspection.

    Detection of chemical composition testing for casting components

About Lantian Precision Machinery Manufacturing Foundry

  1. 30 Years of Rich Experience  Investment Casting Foundry.
    Lantian Precision Machinery Manufacturing Company is a professional invesment casting foundry in China for 30 years. We can produce stainless steel castings, carbon steel castings, alloy steel castings and high-precision components according to standards.
  2. 4 Branch Factories
    Presently we have 4 branch factories covering an area of 19,000m2 on production of casting products. Total over 400 staff working in our foundry.
  3. Passed the ISO 9001:2000 in 2003 and TS 16949:2002 Certification in 2008.
    Our company passed the ISO 9001:2000 quality management system certification in January 2003.  In March 2008, we obtained the TS 16949:2002 quality management system certificate,  and we have obtained the production license issued by the Germanischer Lloyd.
  4. Top 10 Brand Hardware Manufacture in China
    In 2006, we were awarded the title of “Top 10 Reputable Enterprises in Liaoning Province” by the reputation committee of Liaoning Province. We always persists on the policy of “High Quality, Customer First, Continuous Innovation, Sustainable Development,” for enterprise management, to meet customer expectations and higher requirements of quality.

Certificates and Honor_LANTIAN FOUNDRY CASTINGS CERTIFICATES

Application of Investment Castings 

  • Industrial Machinery: Gears, shafts, bearings, housings, and other critical components.
  • Automotive: Engine parts, transmission components, suspension systems, and chassis parts.
  • Construction: Structural steel components, fasteners, brackets, and custom fittings.
  • Agriculture: Heavy-duty equipment parts, tillage tools, and harvesting components.
  • And Many More!

Your Trusted Partner for  Investment Castings:

At Lantian Precision Machinery Manufacturing Co.,Ltd, we are committed to providing you with the highest quality custom steel components and exceptional service. Your business will be safe with our company and your money is safe too!

Website: www.ltsteelcasting.com

Whatsapp: 0086-13478609753

Email:ltcasting@hotmail.com

Get Quote